Instruction for Infilled Material of “JECC-UNITEC” Steel Raised Floor
 May 30, 2013|View:284

(1) Inside cavity is filled with avirulent Portland cement No.425.  Performances of Cement, such as strength, consolidation, fine granulation, safety, are all in accordance with requirements and index specified by National Inspection Department.

 

(2) The density of foam cement is up to 1.2g/cm3 after adding slurry, and foam fine particles are compact and distributed uniformly. Make sure inside cavity is completely filled after adding slurry.

 

(3) After adding slurry, the bare steel panel should be put aside for 28 days under the temperature of 25℃-30℃ as a cement curing period in winter.

 

(4) Foam cement after adding slurry should be prevented from coaly debris, reinforcing steel bar and any other harmfully inferior materials. 